Get A quote
Inquiry
Form loading...
ZYTC Alloy® Ships INVAR 36 Sheet to Taiwan: ASTM F1684 Quality, Full Traceability, and 20 Years of Export Excellence
Company News

ZYTC Alloy® Ships INVAR 36 Sheet to Taiwan: ASTM F1684 Quality, Full Traceability, and 20 Years of Export Excellence

2026-10-29

Invar 36: The Low-Expansion Alloy Behind Precision That Cannot Afford to Move

INVAR 36 (UNS K93600 / K93603, W.Nr. 1.3912) is a nickel–iron controlled-expansion alloy containing approximately 36% nickel, with the balance iron. Its defining characteristic is an extremely low coefficient of thermal expansion (CTE) near room temperature—roughly one-tenth that of carbon steel—which allows components to maintain dimensional stability across temperature swings that would distort ordinary metals. That property makes INVAR 36 indispensable in aerospace tooling, precision optics, laser systems, measurement standards, cryogenic equipment, and composite molds.

ZYTC Alloy® has just completed an export order of INVAR 36 Sheet to Taiwan, produced to Astm F1684, sized 0.3 × 519 × 600 mm. The shipment followed a fully standardized, process-driven route—melting, forging, rolling, nondestructive testing, inspection, packaging, and dispatch—with ZYTC and third-party supervision at every stage. Pre-shipment samples were sent to the customer for verification, and the material was released only after passing acceptance testing.


Chemical Composition of INVAR 36 (ASTM F1684)

Element Composition Limit (wt. %) Role
Ni 35–38 Establishes the Invar effect
Fe Balance Matrix
C 0.10 max Controls carbide formation
Mn 0.06 max Deoxidation / residual control
Si 0.35 max Residual control
P 0.025 max Impurity limit
S 0.025 max Impurity limit
Cr 0.50 max Residual allowance
Mo 0.50 max Residual allowance
Co 1.0 max Residual allowance

Source: ASTM F1684 composition limits as published in alloy technical data

The 36% Ni window is intentionally narrow: falling below it weakens the magnetovolume contribution responsible for low expansion, while exceeding it begins to raise CTE again. That is why INVAR 36 chemistry control is inseparable from expansion performance.


Invar 36 Mechanical and Physical Properties 

Property Annealed Condition Notes
Ultimate Tensile Strength ≈ 490 MPa (71 ksi) Typical for sheet / plate
Yield Strength (0.2%) ≈ 240–310 MPa Depending on product form and test direction
Elongation ≥ 30% (typically ~40%) Good ductility for forming
Hardness ≤ 135–140 HB Annealed, descaled
Density 8.05 g/cm³
Elastic Modulus ≈ 141 GPa Lower than stainless steel
Curie Temperature ≈ 230 °C Above this, low-CTE behavior degrades
CTE (20–100 °C) ≈ 1.2 × 10⁻⁶ /°C The signature property

Data consolidated from ASTM F1684-referenced property tables and alloy datasheets

INVAR 36 is ferromagnetic at room temperature, and its low thermal expansion is a magnetovolume phenomenon—not merely a compositional accident. Designers specifying INVAR 36 for dimensional stability should therefore treat the Curie temperature as a hard boundary: above roughly 230 °C, the alloy loses its anomalous expansion behavior and CTE rises sharply.


INVAR 36 vs. KOVAR: Different Problems, Different Alloys

Both are controlled-expansion alloys, but they are not interchangeable. INVAR 36 is an iron–nickel binary optimized for near-zero expansion; KOVAR® is an iron–nickel–cobalt alloy (approximately 29% Ni, 17% Co) engineered to match the expansion of borosilicate glass and hard ceramics for hermetic seals.

Comparison Point INVAR 36 KOVAR®
Base system Fe–36Ni Fe–29Ni–17Co
CTE (typical) ≈ 1.2 ppm/°C (20–100 °C) ≈ 5.3 ppm/°C
Expansion-matching target Near-zero expansion / carbon-fiber composites Borosilicate glass, alumina ceramics
Primary function Dimensional stability Glass-to-metal / ceramic-to-metal sealing
Typical use Aerospace composite tooling, optical benches, laser housings, length standards Hermetic packages, electron tubes, feedthroughs, sensor seals
Expansion mechanism Magnetovolume (Invar effect) Compositional CTE matching to glass/ceramic

The CTE gap is decisive: INVAR 36 at about 1.2 ppm/°C is roughly one-quarter the expansion of KOVAR® at about 5.3 ppm/°C. Specifying KOVAR® where INVAR 36 is required sacrifices dimensional stability; specifying INVAR 36 for a glass-seal joint creates a CTE mismatch. ZYTC Alloy® supplies both families and helps customers route the specification correctly before the order is released.


Where INVAR 36 Is Used

INVAR 36 earns its place in systems where a few micrometres of thermal movement can ruin function:

  • Aerospace composite tooling — layup molds and fixtures that must hold tolerance against carbon-fiber prepreg CTE

  • Precision optics and laser systems — optical benches, mirror substrates, and laser housings requiring low thermal expansion

  • Measurement and reference standards — length standards, gauge blocks, tape measures, and metrology frames

  • Cryogenic components — LNG tank membranes and cryocooler hardware where INVAR 36 retains useful toughness and stability

  • Thermostatic and bimetallic devices — INVAR 36 paired with a higher-expansion metal to actuate temperature-responsive elements


How ZYTC Alloy® Delivers INVAR 36 Quality

ZYTC Alloy® brings 20 years of export experience in nickel-based alloys, cobalt-based alloys, titanium, and controlled-expansion materials. For this INVAR 36 Sheet order, the production route was fixed from the start: melting → forging → rolling → nondestructive testing → inspection → packaging → shipment, with ZYTC and third-party oversight throughout.

The company operates an independent laboratory capable of chemical composition analysis, mechanical property testing, impact energy, high-temperature properties, grain size, and stress-rupture testing. ZYTC Alloy® is certified to ISO 9001 and AS9120B, the aerospace-focused distribution standard. INVAR 36 is available as sheet, plate, tube, strip, forging, and capillary tubing, and the team can work from customer drawings while executing to ASTM, AISI, ISO, JIS, and AMS requirements.

The value proposition is straightforward: fast delivery, reasonable pricing, and high quality—backed by documented process control rather than promises. Customers receive pre-shipment samples, third-party verification where required, and full traceability from melt to dispatch.


Frequently Asked Questions

Q: What is the difference between INVAR 36 and KOVAR® in one sentence?
INVAR 36 is optimized for near-zero thermal expansion; KOVAR® is optimized for matching the expansion of glass and ceramics for hermetic seals. Their CTEs—about 1.2 ppm/°C versus 5.3 ppm/°C—reflect that different design intent.


Q: Does ZYTC Alloy® supply INVAR 36 only in sheet?
No. INVAR 36 is available from ZYTC Alloy® as plate, sheet, strip, tube, forging, and capillary tubing. The 0.3 × 519 × 600 mm sheet shipped to Taiwan is one specification among a broader product range.


Q: What standard governs the INVAR 36 shipment described here?
This order was produced to ASTM F1684, the standard specification covering INVAR 36 controlled-expansion alloy. ZYTC Alloy® also works to AISI, ISO, JIS, AMS, and customer drawings.


Q: Can ZYTC Alloy® provide third-party inspection for INVAR 36?
Yes. The Taiwan shipment was supervised by ZYTC and a third party throughout production and inspection. Pre-shipment samples were sent to the customer, and release followed successful customer acceptance testing.


Q: Why does INVAR 36 stop being “INVAR” above a certain temperature?
The low-CTE behavior depends on the Invar magnetovolume effect, which fades near the Curie temperature (≈ 230 °C). Above that point, INVAR 36 expands more like a conventional alloy, so designs should not assume near-zero expansion outside the specified range.

画板 1.jpg

画板 2.jpg

画板 3.jpg

画板 4.jpg

画板 5.jpg