L605, also known as Haynes® 25, Udimet® L605, or UNS R30605, is a non-magnetic cobalt-based superalloy that delivers exceptional performance in high-temperature and corrosive environments. As a Cobalt-Chromium-Tungsten solid-solution strengthened alloy, L605 combines excellent mechanical strength with outstanding oxidation resistance at elevated temperatures. This remarkable cobalt alloy has become the material of choice for aerospace, land-based turbines, power generation, electronics, and medical applications.

Chemical Composition of L605

The nominal chemical composition of L605 (Haynes 25) is precisely controlled to deliver its superior properties:

Element Weight %
Cobalt (Co) Balance
Chromium (Cr) 19.0 – 21.0
Tungsten (W) 14.0 – 16.0
Nickel (Ni) 9.0 – 11.0
Manganese (Mn) 1.0 – 2.0
Iron (Fe) 3.0 max
Silicon (Si) 0.40 max
Carbon (C) 0.05 – 0.15
Phosphorus (P) 0.040 max
Sulfur (S) 0.030 max

This carefully balanced cobalt-nickel-chromium-tungsten formulation gives L605 its renowned high-temperature strength and resistance to oxidation and carburization.

Physical Properties of L605

Property Value
Density 0.335 lb/in³ (9.27 g/cm³)
Modulus of Elasticity 32.6 × 10³ ksi (225 GPa)
Melting Range 2426 – 2570 °F (1300 – 1410 °C)
Electrical Resistivity 34.9 µΩ·in (88.6 µΩ·cm)
Thermal Conductivity 65.0 Btu-in/ft²hr-°F (9.4 W/m-K)

L605 exhibits excellent resistance to oxidation and carburization up to 1900°F (1038°C), and can withstand continuous service up to 2000°F (1093°C). The alloy also demonstrates outstanding resistance to sulphidation, wear, and galling.

Mechanical Properties of L605

L605 (Haynes 25) offers impressive mechanical properties that make it ideal for demanding applications:

Condition Tensile Strength Yield Strength (0.2% offset) Elongation
Annealed 130 – 180 ksi (896 – 1240 MPa) 55 – 80 ksi (379 – 552 MPa) 41%
Cold Worked 220 – 280 ksi (1517 – 1930 MPa) – –

Alloy L-605 can only be significantly hardened through cold working. Cold working enhances creep strength up to 1800°F and stress rupture strength up to 1500°F.

Applications of L605

L605 (UNS R30605) is widely utilized across multiple industries:

Aerospace & Gas Turbines:

  • Combustor liners

  • Gas turbine rotors

  • Turbine rings and blades

  • Combustion chamber components

  • Nozzle diaphragm valves

  • Jet engine components

  • Seal rings

Industrial Applications:

  • Furnace liners and mufflers

  • High-temperature kiln components

  • High-temperature ball bearings and races

Medical & Other:

  • Heart valves

  • Surgical fixation wire

  • Springs

L605 Product Forms & Specifications

ZYTC Alloy manufactures and supplies L605 in a comprehensive range of product forms:

Product Form Applicable Specification
Sheet, Strip, Plate AMS 5537
Bar, Forging Stock, Forgings, Rings AMS 5759
Welding Wire AMS 5796
Welding Rod AMS 5797 (UNS W73605)
Bar and Wire (Surgical Implant Quality) ASTM F90
Various Forms W.Nr 2.4964 / 2.4967

Our L605 products strictly comply with ASTM, EN, and AMS standards. We offer custom manufacturing and machining services according to customer drawings, ensuring precision and quality for every application.

Recent Success: L605 Forging Ring Shipment to Turkey

ZYTC Alloy recently completed and successfully delivered an order of L605/Haynes 25/UNS R30605 Forging Rings to Turkey. The forging ring was manufactured to specification Ф300 × Ф230 × 10mm under the stringent AMS 5759N standard, with solution and turned finish delivery condition.

Our company has standardized, process-driven, and professional production and inspection procedures. The product underwent comprehensive testing and finally passed SGS inspection before delivery, ensuring full compliance with international quality requirements.

Why Choose ZYTC Alloy for L605?

  • Complete Product Line: L605 sheet, strip, wire, bar, tube, forging, and related products

  • Strict Standard Compliance: AMS 5537, AMS 5759, AMS 5796, AMS 5797, ASTM F90

  • Custom Manufacturing: Available for custom machining and forging according to drawings

  • Fast Delivery: Competitive lead times

  • Competitive Pricing: Cost-effective solutions without compromising quality

  • Quality Assurance: Rigorous SGS inspection and testing protocols

Contact ZYTC Alloy today for your L605 (Haynes 25 / UNS R30605) requirements – from high-temperature superalloy components to precision forgings and rings.

画板 1.jpg

画板 2.jpg

画板 3.jpg

画板 4.jpg

画板 6.jpg