Alloy 230 Nickel Superalloy: AMS 5878E Grade for Aerospace & Power Generation – Delivered to Turkey
ZYTC Alloy proudly announces the successful completion and delivery of an export order of Alloy 230 (UNS N06230) nickel sheet to Turkey, produced to the AMS 5878E standard. The material was supplied in dimensions of 2.0 × 1000 × 2000 mm, fully inspected and certified as qualified before final release to our valued customer.
At ZYTC Alloy, every stage of production and inspection adheres strictly to the core principles of Standardization, Process Optimization, and Professionalism. Our dedicated quality assurance team implements rigorous testing protocols, ensuring that every product—including this recent shipment of Alloy 230 sheet—meets or exceeds international specifications. Before any material leaves our facility, it undergoes comprehensive final testing to confirm full compliance with customer requirements.
Alloy 230 (Uns N06230), also known commercially as Haynes 230, is a nickel-chromium-tungsten-molybdenum superalloy designed for extreme operating environments. It is a solid-solution strengthened alloy that delivers an unmatched combination of high-temperature strength, oxidation resistance, long-term thermal stability, and nitriding resistance .
📌 Chemical Composition of Alloy 230 (UNS N06230)
The superior properties of Alloy 230 derive from its carefully balanced chemical design. Below is the nominal chemical composition of UNS N06230:
| Element | Wt. % (Nominal Range) |
|---|---|
| Nickel (Ni) | 47.00 – 65.00 (Balance) |
| Chromium (Cr) | 20.00 – 24.00 |
| Tungsten (W) | 13.00 – 15.00 |
| Molybdenum (Mo) | 1.00 – 3.00 |
| Cobalt (Co) | up to 5.00 (max) |
| Iron (Fe) | up to 3.00 (max) |
| Silicon (Si) | 0.25 – 0.75 |
| Manganese (Mn) | 0.30 – 1.00 |
| Aluminum (Al) | 0.20 – 0.50 |
| Carbon (C) | 0.05 – 0.15 |
| Lanthanum (La) | 0.005 – 0.05 |
The addition of tungsten (up to 15%) provides solid-solution strengthening, while chromium enhances oxidation resistance. The precise lanthanum addition contributes to superior scale adhesion at extreme temperatures.
📌 Mechanical Properties of Alloy 230 (UNS N06230) – AMS 5878E Compliant
Alloy 230 exhibits outstanding mechanical properties across a wide temperature range, making it one of the most robust nickel-based superalloys available. The table below summarizes typical mechanical properties for Alloy 230 in the annealed condition, as supplied under AMS 5878E and ASTM B435:
| Mechanical Property | Value (Typical) |
|---|---|
| Tensile Strength, Ultimate | 758 – 965 MPa (110 – 140 ksi) |
| Tensile Strength, Yield (0.2% offset) | 310 – 450 MPa (45 – 65 ksi) |
| Elongation at Break | 30 – 44% (in 5D or 50 mm gauge length) |
| Hardness | 150 HB ~ 30 – 36 HRC |
| Density | 8.97 – 9.05 g/cm³ |
In addition to its room-temperature strength, Alloy 230 offers exceptional long-term stability at elevated temperatures, with excellent creep resistance and thermal fatigue resistance, making it particularly effective for very long-term service at 650°C (1200°F) and above .
🔩 Physical Properties
Beyond its mechanical performance, Alloy 230 offers a combination of physical properties that enhance its suitability for extreme environments:
-
Density: 0.324 – 0.327 lb/in³ (8.97 – 9.05 g/cm³)
-
Melting Range: 1360 – 1410°C (2480 – 2570°F)
-
Modulus of Elasticity (E) : 30.3 – 30.6 × 10³ ksi (209 – 211 GPa) at room temperature
-
Coefficient of Thermal Expansion: 8.9 µin/in-°F (70–1800°F) / 16.1 µm/m-°C (25–1000°C)
-
Electrical Resistivity: 49.2 µΩ·in (125.0 µΩ·cm)
-
Thermal Conductivity: 62 Btu-in/ft²-hr-°F (8.9 W/m·K)
-
Magnetic Permeability: ~1.00 (non-magnetic)
Notably, Alloy 230 exhibits lower thermal expansion characteristics than most high-temperature alloys and demonstrates pronounced resistance to grain coarsening with prolonged exposure to high temperatures .
🏭 Applications and Industries Served
Thanks to its exceptional high-temperature strength and outstanding oxidation resistance up to 1149°C (2100°F) for prolonged exposures, Alloy 230 is widely specified across demanding industries [10†L7-L9].
Aerospace & Power Generation
Alloy 230 is extensively used in gas turbines for components such as:
-
Combustion cans and combustor liners
-
Transition ducts
-
Flameholders
-
Thermocouple sheaths
-
Hot section rings, seals, and shrouds
The alloy demonstrates superior creep resistance, making it ideal for gas turbine engines and advanced power generation systems [2†L29-L31].
Chemical Processing & Industrial Heating
In the chemical process industry, Alloy 230 serves critical functions including:
-
Catalyst grid supports in ammonia burners
-
High-strength thermocouple protection tubes
-
High-temperature heat exchangers
-
High-temperature bellows
-
Ducts and varied process internals
Industrial heating applications for Alloy 230 include furnace retorts, chains and fixtures, burner flame shrouds, recuperator internals, dampers, nitriding furnace internals, heat-treating baskets, grates, trays, sparger tubes, cyclone internals, and more.
Industries Supplied
ZYTC Alloy supplies Alloy 230 products to the following industries:
-
✈️ Aerospace
-
⚡ Power Generation
-
🏭 Industrial Heating
-
🧪 Chemical Processing
-
🔧 Thermal & Petrochemical Processing
🔧 Product Forms and Manufacturing Capabilities
At ZYTC Alloy, we are capable of producing Alloy 230 in a comprehensive range of forms to meet diverse application requirements:
🔹 Alloy 230 Sheet & Plate
🔹 Alloy 230 Strip & Coil
🔹 Alloy 230 Bar & Rod
🔹 Alloy 230 Wire
🔹 Alloy 230 Tube & Pipe
🔹 Alloy 230 Forgings
🔹 Custom products to customer drawings
We can process custom sizes, cutting, and fabrication to meet your exact specifications. All products undergo strict testing and quality control to ensure compliance with your required standards.
⚙️ Compliance with Global Standards
ZYTC Alloy produces Alloy 230 products in full compliance with major international specifications:
-
ASTM (American Standards) – including ASTM B435
-
EN (European Norms)
-
AMS (Aerospace Material Specifications) – including AMS 5878E
Our commitment to standardization means you receive Alloy 230 materials that meet the most demanding quality and performance requirements, ready for deployment in critical applications worldwide.
🚢 Why Choose ZYTC Alloy for Your Alloy 230 Requirements?
✓ Fast delivery – Streamlined production and logistics keep your projects on schedule
✓ Reasonable pricing – Competitive rates without compromising quality
✓ Superior quality – Stringent testing and inspection protocols guarantee product integrity
✓ Full product range – Sheet, strip, wire, bar, tube, pipe, and forgings
✓ Customization – Manufactured to your drawings and specifications
✓ Global compliance – ASTM, EN, AMS standards verified
✓ Proven track record – Successfully exported to Turkey and many other countries worldwide